Heat treatment of metals · Maribor, Slovenia
Stress relief annealing of weldments up to 100 t
Four industrial furnaces that take parts up to 12.8 metres long. A controlled heat treatment cycle and an annealing chart for every weldment, before it goes to machining.
What we do
Your partner for heat treatment of weldments
You deliver the weldment, we crane it into the furnace, anneal it to the specified cycle and load it back onto your truck.
All about annealing
01Stress relief annealingReducing residual stresses after welding, before machining.
02Furnaces and capacitiesFour furnaces up to 12.8 m long and 100 t load capacity.
03Measurement and chartsAutomatic control, thermocouples on the part, a chart for every cycle.
04Quality and certificatesISO 9001, ISO 14001, SGS and DNV.
Controlled process
Precise cycle. Documented result.
Multi-zone control
The furnace heating zones are controlled separately, so even a heavy part with varying wall thicknesses heats up more evenly.
Automatic control
Heating, soaking and cooling follow a set programme that is repeated identically in every cycle.
Thermocouples on the part
In furnaces 3 and 4 we measure the temperature directly on the weldment, with up to 12 thermocouples.

Annealing chart
A chart is generated automatically after every cycle. With thermocouple measurement you also receive a report.
20 t and 64 t cranes
We do the loading and unloading ourselves, even for the heaviest parts.
Our own solar plant
A 156.6 kWp solar plant and a 1305 kWh battery cover part of the furnaces’ energy use.
Our furnaces
Four furnaces for every size of weldment
We choose the furnace by dimensions, weight and the required cycle. Send us the drawing and we will check which one fits.
- W × H
- 3.4 × 3.6 m
- Depth
- 12.0 m
- Max. temperature
- 650 °C
- W × H
- 3.0 × 2.7 m
- Depth
- 4.4 m
- Max. temperature
- 580 °C
- W × H
- 5.3 × 4.0 m
- Depth
- 6.4 m
- Max. temperature
- 650 °C
- W × H
- 3.9 × 4.5 m
- Depth
- 12.8 m
- Max. temperature
- 750 °C
Furnace floor plans drawn to the same scale, 1 m grid.
How it works
From enquiry to collection
You get the exact date with your quotation. When we are not fully booked, a part is usually ready in 2 to 3 days.
Send an enquiry- 1
Enquiry
Send us the drawing, weight, material and the required heat treatment cycle.
- 2
Delivery on schedule
We accept vehicles up to 30 m long and 6 m wide.
- 3
Annealing
Heating, soaking at temperature and controlled cooling.
- 4
Chart and collection
We load the part onto your truck and hand over the annealing chart.
Temperature cycle
Every cycle is recorded in a chart
We heat the part gradually, hold it at the required temperature and cool it in a controlled way. The cycle is recorded automatically in the annealing chart, which you receive together with the part.
In furnaces 3 and 4 we also measure the temperature directly on the material, with up to 12 probes.
How annealing works
FAQ
What customers ask first

Does stress relief annealing remove all residual stresses?
Can annealing prevent distortion during machining?
How quickly can you anneal?
Do I receive an annealing chart?
What information do you need for a quotation?
Enquiry
You send the drawing. We choose the right furnace.
Dimensions, weight and material are enough for us to check which furnace fits and confirm a date.
Send an enquiry